Standard |
|
| |
It is According to ASTMC 494 types A, F,
BS 5075 part T3 standard |
|
| |
 |
Advantages |
|
 |
|
Increase strength without addition of
cement at primary steps |
 |
|
It is chlorine free, which does not damage to
reinforcement |
 |
|
Increasing concrete efficiency without
additional water |
 |
|
Decreasing shrinkage and creep of concrete |
 |
|
Increase of primary and final resistance |
|
| |
 |
Uses |
|
 |
|
For manufacture of concrete with high efficiency and
high strength |
 |
|
For concretes and prefabricate element |
 |
|
For freezing or high temperature conditions |
 |
|
Slabs and columns |
 |
|
Amount of consumption |
|
| |
 |
Amount of consumption |
|
 |
|
For obtain high strength, normal range of consumption
is about 0.70 1.5 liter per 100 kg of cement |
|
| |
 |
storage |
|
 |
|
If it is kept far from cold and warm condition, and
in range of 5 2 temperature, the life time of this material
would be about 12 months |
|
| |
 |
Safety |
|
 |
|
It is not high toxic, but must not contact with eye,
skin, and
respiratory system |
|
Contact Us
E-mail
Us
|
|
 |
Standard |
|
| |
It is according to ASTMC- 494 Type G , BS
5075 part 3 |
|
| |
 |
Advantages |
|
 |
|
Increasing the concrete efficiency in hot
climate |
 |
|
Increasing the compressive strength of concrete without
increasing cement |
 |
|
Chlorine free which does not effect &
damages to reinforcement |
 |
|
Controlling of air content in concrete |
 |
|
Improvement external facing of concrete |
|
| |
 |
Uses |
|
 |
|
Suitable for hot climate |
 |
|
Suitable for high quality concrete |
|
| |
 |
Amount of consumption |
|
 |
|
0.7 to 1.5 liter of compound per 100 kg of cement |
|
| |
 |
storage |
|
 |
|
12 months from producing in ambient condition (15 to
45) 0c |
|
| |
 |
Safety |
|
 |
|
This component is non-toxic, but should not contact to
eyes, skin&
Should not be swallowed |
|
Contact Us
E-mail
Us
|
|
| Additive plasticizer, late freeze and
decreasing of water |
 |
Standard |
|
 |
|
t is according to B, ASTMC 494D, BS 5075
standard |
|
| |
 |
Advantages |
|
 |
|
It increases ultimate strength
of concrete. |
 |
|
improved efficiency of concrete without
Increasing of water. |
 |
|
Without setting, it accelerates
hardness of concrete. |
 |
|
Increasing working time of concrete |
 |
|
Improvement trowel. |
 |
|
Economic in use of cement |
 |
|
Decreasing water, without decrease in
efficiency |
 |
|
Increase freezing time in hot climate. |
|
| |
 |
Uses |
|
 |
|
At High temperature |
 |
|
In continuous pouring of concrete, used for big
surfaces. |
 |
|
For concrete in external facing surfaces. |
 |
|
For ready mixed concrete. |
|
| |
 |
Amount of consumption |
|
 |
|
0.6 0.8 liter per 100 kg of cement. |
|
Contact Us
E-mail
Us
|
|
| Water increasing additive, Lingo sulfate base
plasticizer. |
 |
Standard |
|
 |
|
It is according to ASTMC 494 TYPEA,, BS 5075 part 1
standard |
|
| |
 |
Advantages |
|
 |
|
Efficiency improvement to
concrete. |
 |
|
iIncreasing concrete strength without
Increase of cement. |
 |
|
It is chlorine free, so does
not damage to reinforcement. |
 |
|
Increase concrete materials adhesiveness. |
 |
|
Improvement of external facing of concrete
for external surfaces. |
|
| |
 |
Uses |
|
 |
|
Plasticizer properties of this compound are important
for following: |
 |
|
When low quality sand and gravel is used for concrete
production. |
 |
|
High efficiency concrete is used. |
 |
|
The concrete have external surface. |
|
| |
 |
Amount of consumption |
|
 |
|
0.3 to 0.42 lit per 100 kg of cement. |
|
Contact Us
E-mail
Us
Concrete admixture ,
Accelerator RB SC3
|
| Accelerators of reinforced concrete for dry
pouring concrete under o.c |
 |
Standard |
|
 |
|
It according to BS 5075 PART,
standard |
|
| |
 |
Advantage |
|
 |
|
Suitable for cold condition
under 16 |
 |
|
It is chlorate free and does not damage to
reinforcement |
 |
|
Accelerating interception of concrete pipe |
 |
|
Decrease wasting materials and accelerating
the process |
 |
|
Increase primary strength of concrete |
 |
|
Prevention of freezing of concrete by air
bubbles |
 |
|
Decrease water amount and fluidity
protection |
|
| |
 |
Uses |
|
 |
|
Suitable for concrete spraying |
 |
|
In cold condition |
 |
|
Suitable for parts of concrete that is
under freezing and cold condition |
|
| |
 |
Amount of consumption |
|
 |
|
2.5 liter per 100 kg |
|
| |
 |
storage |
|
 |
|
Optimum condition for storage is in
original barrels, in this condition, the life time of this compound is
about 12 months |
|
Contact Us
E-mail
Us
|
|
Accelerator for reinforced concrete for under 0
temperature
|
 |
standard |
|
 |
|
According to BS 5075 Part1 |
 |
|
ASTM c-494 standard |
|
| |
 |
Advantage |
|
 |
|
Concrete and mortar plasticizer |
 |
|
Suitable for operation under 0
temperature |
 |
|
Acceleration initial
interception |
 |
|
Creation of strength quickly |
 |
|
Decrease of seed separation |
|
| |
 |
Uses |
|
 |
|
Suitable for cold region that
is under freezing or under 0 temperature |
 |
|
In Tunnels |
 |
|
Suitable for prefabricated element of
concrete |
|
| |
 |
Amount of consumption |
|
 |
|
2.6 liter per 100 kg cement, under (-2)
-(4) temperature |
 |
|
3.4 liter per 100 kg cement, under -2
temperature |
|
Contact Us
E-mail
Us
|
|
| Producer of air bubble in concrete |
 |
Standard |
|
 |
|
According to ASTMC 260 66T |
|
| |
 |
Advantage |
|
 |
|
Creation and homogeneous
distribution of air bubble in concrete mixtures for Increase freezing
and high temperature strength of concrete |
 |
|
It is free from chlorine, thus is safe for
reinforcement |
 |
|
It Increase concrete efficiency |
 |
|
It Increase concrete compression |
 |
|
It decreases separation of seeds and
shrinkage |
 |
|
It Increase concrete fluidity |
 |
|
Decreasing permeability and improvement of
waterproofing concrete as a result |
|
| |
 |
Uses |
|
 |
|
Roads |
 |
|
Heavy concrete structural |
 |
|
Dams and water storage |
 |
|
Airport Bonds |
|
| |
 |
Amount of consumption |
|
 |
|
Consumption of AB AE is related to air
bubble for concrete preparation design. This amount is between0/1 to 0.5
percent of cement |
|
| |
 |
storage |
|
 |
|
If it keeps in original barrels and 5-70 ,
life time will be 12 to 18 months |
|
.htm_txt_icon_todays_new[1]_7.gif)
Need more
information?
Click here to contact us!
Contact Us
E-mail
Us
|